Comparison
Prusament TPU 95A vs eSUN 3D TPU-95A
The tiles and the table are the listed numbers. Source wording sits under Sources & notes.
Prusament TPU 95A
- Nozzle220–240 °C
- Bed55–75 °C
- SpeedNot listed
- Dry—
- Density1.22 g/cm³
eSUN 3D TPU-95A
- Nozzle210–240 °C
- Bed30–60 °C
- SpeedNot listed
- Dry—
- Density1.2 g/cm³
Side by side
| Spec | Prusament TPU 95A | eSUN 3D TPU-95A |
|---|---|---|
| Material | TPU | TPU |
| Nozzle temperature | 220–240 °C | 210–240 °C |
| Bed temperature | 55–75 °C | 30–60 °C |
| Print speed | Not listed | Not listed |
| Drying | Not listed | Not listed |
| Enclosure required | Not listed | Not listed |
| Chamber temperature | ideal 30 °C and maximum 40 °C | Not listed |
| Hardened nozzle | Not listed | Not listed |
| Spool weight | 500 g | 1 kg (1000 g) |
| Price per kg | Not listed | Not listed |
Sources & notes
Prusament TPU 95A lists a recommended nozzle temperature of 220–240 °C and a recommended bed temperature of 55–75 °C, according to the Open Filament Database (record https://api.openfilamentdatabase.org/api/v1/brands/prusament/materials/TPU/filaments/tpu_95a/index.json; dataset verified date 2026-10-13). eSUN 3D TPU-95A lists a recommended nozzle temperature of 210–240 °C and a recommended bed temperature of 30–60 °C, according to the Open Filament Database (record https://api.openfilamentdatabase.org/api/v1/brands/esun_3d/materials/TPU/filaments/tpu_95a/index.json; dataset verified date 2026-10-13). Where a source leaves a value blank, this comparison leaves it blank.
Questions
What nozzle temperatures are listed for Prusament TPU 95A vs eSUN 3D TPU-95A?
Prusament TPU 95A lists 220–240 °C. eSUN 3D TPU-95A lists 210–240 °C.
What bed temperatures are listed for Prusament TPU 95A vs eSUN 3D TPU-95A?
Prusament TPU 95A lists 55–75 °C. eSUN 3D TPU-95A lists 30–60 °C.