Comparison
TPU 95A vs TPU 85A
The tiles and the table are the listed numbers. Source wording sits under Sources & notes.
Prusament TPU 95A
- Nozzle220–240 °C
- Bed55–75 °C
- SpeedNot listed
- Dry—
- Density1.22 g/cm³
Bambu Lab TPU 85A
- Nozzle200–250 °C
- Bed30–35 °C
- SpeedNot listed
- Dry70 °C maximum
- Density1.18 g/cm³
Side by side
| Spec | Prusament TPU 95A | Bambu Lab TPU 85A |
|---|---|---|
| Material | TPU | TPU |
| Nozzle temperature | 220–240 °C | 200–250 °C |
| Bed temperature | 55–75 °C | 30–35 °C |
| Print speed | Not listed | Not listed |
| Drying | Not listed | 70 °C maximum |
| Enclosure required | Not listed | Not listed |
| Chamber temperature | ideal 30 °C and maximum 40 °C | Not listed |
| Hardened nozzle | Not listed | Not listed |
| Spool weight | 500 g | 1 kg (1000 g) |
| Price per kg | Not listed | Not listed |
Sources & notes
Prusament TPU 95A lists a nozzle of 220–240 °C and a bed of 55–75 °C. Bambu Lab TPU 85A lists a nozzle of 200–250 °C and a bed of 30–35 °C. 95A is the stiffer of the two Shore A values. Shore hardness is the grade in the product name, not a second temperature.
Questions
What nozzle temperatures are listed for TPU 95A vs TPU 85A?
Prusament TPU 95A lists 220–240 °C. Bambu Lab TPU 85A lists 200–250 °C.
What bed temperatures are listed for TPU 95A vs TPU 85A?
Prusament TPU 95A lists 55–75 °C. Bambu Lab TPU 85A lists 30–35 °C.